Temperable Mirror Toughening Parameters (Reference Only) |
|
|
The top temperature |
675℃—680℃ |
|
The bottom temperature |
670℃—675℃ |
|
Heating time |
5mm 225—250S |
|
convection(Upper) |
Heating Time |
|
Section 1 |
30% 5Hz |
|
Section 2 |
25% 6Hz |
|
Section 3 |
45% 8Hz |
|
Note: |
1) 5-10℃lowerinfrontandbackthaninmiddlefurnace. |
|
2) Conacting with corrosive chemicals is not allowed. |
|
|
3) Cleaning by soft brush&neutral water. |
|
|
4) Removing the stains on coatting by alcohol. |
|